Recipe

Small type and badges

Keeping names sharp when art gets tiny.

Small type and badges

I am often asked how to keep those tiny badge names and school numbers looking crisp with DTF, especially when the artwork pushes the limits of what the process can hold. In badge and name printing, every dot of ink counts, and so does the way you handle powder and film. I have spent a lot of time testing small-type runs in our Meadowdale lab and have picked up a few points that consistently help keep small detail sharp.

Start with the right artwork and RIP settings

To get clean small lettering, start with crisp vector art or high-resolution raster images, no blurry jpegs or soft-edged exports. Text below 7 pt in pixel terms often struggles, so check your artwork at real print size before sending it to the RIP. When setting up your white underbase, avoid heavy choking or choking set too wide: a 0.2 to 0.3 mm choke usually helps prevent white halos, but any more can start to close in small counters or lose thin shapes.

In your RIP, use the finest available quality mode and turn off any forced smoothing or anti-aliasing filters that try to 'soften' the art. These can blur tiny letters and bleed them into the fabric texture. If you often print the same badge layout, save a tested RIP preset for quick setup.

Choose a fine film and matching powder

Double-matte PET film is the usual choice for badges and name tags. The matte surface grips the powder evenly and helps with straight feeding in small runs. Store your film flat and sealed, away from moisture, to prevent warping or static. For fine type, always use the soft-hand grade of TPU powder. Coarser grades can create grainy edges, especially where letters are close together.

If you are powdering by hand, wear gloves and shake off all the excess, powder clumps will blur detail and fill small gaps. A small paintbrush can help flick away stray powder from inside closed letters, like 'e' or 'a'.

  • Double-matte PET film helps reduce static and feed issues
  • Soft-hand powder holds fine lines and curves crisply
  • Store film sealed and flat to avoid static and dust

Dial in curing and pressing for sharp edges

Getting sharp edges on small text is just as much about curing as it is about art and powder. Cure the powder in an oven at 110 to 120 degrees C for about 2 to 3 minutes if you have one, or hover under an open press at 145 degrees C for 3 to 4 minutes with a 5 mm gap above the print. Check for a fine orange-peel gloss with no glassy or sticky patches.

When pressing, start with 10 to 12 seconds at 155 degrees C and medium pressure for cotton. For polyester, keep it to 130 degrees C and 12 seconds, then cold peel once fully cool. A quick 5-second finishing press with a Teflon sheet can lock the print in and soften the feel. Always check the press platen with an infrared thermometer for cold spots, uneven heat can cause partial release or blurry edges on small graphics.

Test, check, and avoid common mistakes

Before any run with new badges or small names, test a sample on an offcut and check every letter at arm's length and close up. Look for missing dots, filled-in spaces, or patchy white, these usually mean too much powder, poor nozzle checks, or static on the film.

On the Highveld in winter, dry air can build static that pulls powder where you do not want it. Wipe the film with a clean anti-static cloth and keep a hygrometer in the room. If you see white breaking up or colours patchy, run a nozzle check and white ink agitation, and repeat after any power cut or restart.

  • Avoid fonts thinner than 7 pt at print size
  • Check for static and dust on film before powdering
  • Always run a nozzle check before starting a detail job
Ms Fatiema Pandy
Ms Fatiema Pandy

Colour and RIP specialist at DTF Ink. Owns colour control, RIP setups and underbase tuning for darks.

Talk to DTF Ink

Tell us about your printer, film, powder and press settings and our team will help you get repeatable transfers. Meadowdale lab in Germiston, plus seven studios.